Creep Testing Machine
Flat specimens made of lead and PE. Specimen cross-section 2x5mm, measured length 25mm. Tensile stress range 5...25N/mm².Table unit for the investigation of the creep behaviour of different materials. Position measurement gauge 0...10mm, resolution 0.01mm.
Experiments above or below room temperature possible with conditioning box
 
Technical Data:
•  Tensile stress range: 5...25N/mm².
•  Material: lead, PE.
•  Cross-section: 2x5mm.
•  Measured length: 25mm.
•  Resolution 0.01mm.
•  Position Measurement.
•  Range: 0...10mm.
 